Material Notes:
Pyrex® sheet provides unique chemical, thermal, mechanical, and optical properties. Available in thicknesses from 3/32 inches to 2.25 inches. Tempering increases temperature and pressure capability. Available as polished and machined glass wafers for use in the MST/MEMS (Micro Systems Technology/Micro-Electrical-Mechanical Systems) technologies. Also available in as powdered/crushed in mesh sizes 4 through 325 and is used for sealing and other applications.Information provided by Corning Incorporated.
Physical Properties Metric English Comments
Density 2.23 g/cc
0.0806 lb/in³
Mechanical Properties Metric English Comments
Hardness, Knoop 418
418
Modulus of Elasticity 62.75 GPa
9101 ksi
Poissons Ratio 0.20
0.20
Shear Modulus 26.1 GPa
3790 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 3.25 µm/m-°C

@Temperature 0.000 - 300 °C
1.81 µin/in-°F

@Temperature 32.0 - 572 °F
Softening Point 821 °C
1510 °F
10<sup>7.6</sup> Poise
Working Point 1252 °C
2286 °F
10<sup>4</sup> Poise
Annealing Point 560 °C
1040 °F
10<sup>13</sup> Poise
Strain Point 510 °C
950 °F
10<sup>14</sup> Poise
Optical Properties Metric English Comments
Refractive Index 1.474

@Wavelength 589.3 nm
1.474

@Wavelength 589.3 nm
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+9 ohm-cm

@Temperature 350 °C
1.20e+9 ohm-cm

@Temperature 662 °F
1.60e+11 ohm-cm

@Temperature 250 °C
1.60e+11 ohm-cm

@Temperature 482 °F
Dielectric Constant 4.1

@Frequency 1e+6 Hz
4.1

@Frequency 1e+6 Hz
Dissipation Factor 0.0050

@Frequency 1e+6 Hz
0.0050

@Frequency 1e+6 Hz