Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.33 g/cc | 0.0840 lb/in³ | |
ITW Devcon Plastic Steel® Metal Repair (A), Dark Grey Information provided by ITW Devcon |
|||
Density | 2.33 g/cc | 0.0840 lb/in³ | |
Devcon Plastic Steel® Putty (A) Epoxy General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. .. |