Material Notes:
General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. Cures at room temperature and forms a tough, durable metallic mass. Can be drilled, tapped, machined or painted. Excellent resistance to oil, gasoline, water and many chemicals. Patch and repair areas where welding or brazing would be undesirable or impossible.Data provided by Ellsworth Adhesives.
Physical Properties Metric English Comments
Density 2.33 g/cc
0.0840 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength, Ultimate 22.2 MPa
3220 psi
ASTM D638
Modulus of Elasticity 5.86 GPa
850 ksi
In Tension; ASTM D638
Flexural Yield Strength 38.6 MPa
5600 psi
ASTM D790
Compressive Yield Strength 57.0 MPa
8260 psi
ASTM D695
Adhesive Bond Strength 19.3 MPa
2800 psi
Adhesive tensile shear strength; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 86.0 µm/m-°C

@Temperature 20.0 °C
47.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.573 W/m-K
3.97 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 121 °C
250 °F
Operating Temperature
Shrinkage 0.060 %
0.060 %
During Cure; ASTM D2566
Electrical Properties Metric English Comments
Dielectric Constant 67.5
67.5
ASTM D150
Dielectric Strength 1.18 kV/mm
30.0 kV/in
ASTM D149
Processing Properties Metric English Comments
Processing Temperature 21.1 °C
70.0 °F
Pot Life 45.0 min

@Temperature 23.9 °C
45.0 min

@Temperature 75.0 °F
Descriptive Properties Value Comments
Coverage per lb. 48 in²
at 1/4 inch thick
Mix Ratio by Volume 2.5 to 1
resin:hardener
Mix Ratio By Weight 9 to 1
resin:hardener