Polymer Property : Density = 0.09335 lb/in³
Polymer Property :
Density =
0.09335 lb/in³
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
2.584
-
2.856
g/cc
0.09335
-
0.1032
lb/in³
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F
Information provided by PEAK Werkstoff GmbH