Polymer Property : Density = 0.110 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 3.05 - 3.15 g/cc
0.110 - 0.114 lb/in³
ASTM D792
Polikim EFALON® B-40 PTFE, 40% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
Density 3.04 g/cc
0.110 lb/in³
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
Density 3.05 g/cc
0.110 lb/in³
Apparent
Gouda Vuurvast AC 85-5 Dense Refractory Brick
Description: Excellent resistance against alkali- and metal slags. A good volume stability at very high temperatures. Application: chemical incinerators, combustion chambers for very high temperatur..
Density 3.05 g/cc
0.110 lb/in³
Apparent
Gouda Vuurvast AK 90 Dense Refractory Brick
Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine..
Density 3.05 - 3.12 g/cc
0.110 - 0.113 lb/in³
molded; ASTM D792
Guarniflon PTFE G416 Polytetrafluoroethylene 40% Bronze, 2% Carbon
PTFE G Special Compound with bronze Properties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard ..
Density 3.05 g/cc
0.110 lb/in³
Schott N-BAF52 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.05 g/cc
0.110 lb/in³
Schott N-BAK4 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.05 g/cc
0.110 lb/in³
Schott N-SF10 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.05 g/cc
0.110 lb/in³
3M Nextel™ 440 Industrial Ceramic Fiber
Chemical composition above is wt%. Crystal phases are gamma alumina + mullite + amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural ap..
Density 3.05 g/cc
0.110 lb/in³
3M Nextel™ BF-30 Woven Fabric 440
Information provided by 3M
Density 3.05 g/cc
0.110 lb/in³
3M Nextel™ BF-20 Woven Fabric 440
Information provided by 3M
Density 3.05 g/cc
0.110 lb/in³
3M Nextel™ BF-40 Woven Fabric 440
Information provided by 3M
Density 3.04 g/cc
0.110 lb/in³
Schott N-KZFS5 Glass
Information Provided by SCHOTT North America, Inc.