Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.05 - 3.15 g/cc | 0.110 - 0.114 lb/in³ | ASTM D792 |
Polikim EFALON® B-40 PTFE, 40% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | Apparent |
Gouda Vuurvast AC 85-5 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. A good volume stability at very high temperatures. Application: chemical incinerators, combustion chambers for very high temperatur.. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | Apparent |
Gouda Vuurvast AK 90 Dense Refractory Brick Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine.. |
|||
Density | 3.05 - 3.12 g/cc | 0.110 - 0.113 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G416 Polytetrafluoroethylene 40% Bronze, 2% Carbon PTFE G Special Compound with bronze Properties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
Schott N-BAF52 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
Schott N-BAK4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
Schott N-SF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
3M Nextel™ 440 Industrial Ceramic Fiber Chemical composition above is wt%. Crystal phases are gamma alumina + mullite + amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural ap.. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
3M Nextel™ BF-30 Woven Fabric 440 Information provided by 3M |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
3M Nextel™ BF-20 Woven Fabric 440 Information provided by 3M |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
3M Nextel™ BF-40 Woven Fabric 440 Information provided by 3M |