Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.13 g/cc | 0.113 lb/in³ | |
Nabaltec SYMULOX® M 72 Synthetic Sintered Mullite The homogeneous phase constitution and very low amount of impurities offers considerable advantages over naturally occurring alumosilicates. The synthesized mullite product shows very good chemical .. |
|||
Density | 3.13 g/cc | 0.113 lb/in³ | ASTM D792 |
3M Dyneon™ CC144/S PTFE, 40% Bronze Filled
(discontinued **) Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon. |
|||
Density | 3.14 g/cc | 0.113 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton EXP 386 Aluminum Titanate REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 3.12 g/cc | 0.113 lb/in³ | |
Schott N-SF14 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.13 g/cc | 0.113 lb/in³ | ASTM C135 |
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be forme.. |
|||
Density | 3.12 g/cc | 0.113 lb/in³ | Part A |
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs.. |
|||
Density | 3.12 g/cc | 0.113 lb/in³ | Part A |
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris.. |
|||
Density | 3.12 g/cc | 0.113 lb/in³ | Part A |
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common.. |
|||
Density | 3.12 g/cc | 0.113 lb/in³ | Part A |
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste Ferrobond-P™ is a steel-filled, structural adhesive putty. Repair or fill metal components, castings, tanks, and magnetic fixtures. Preferred to Metalfix-P™ where heavier weight, magnetism, or hig.. |
|||
Density | 3.12 g/cc | 0.113 lb/in³ | Part A |
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra.. |