Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0800 - 0.120 g/cc | 0.00289 - 0.00434 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |