Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0801 g/cc | 0.00289 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ C122A Neoprene/SBR Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | ASTM D1622 |
SABIC Innovative Plastics ULTEM Foam XP080 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | ASTM D1622 |
SABIC Innovative Plastics ULTEM Foam XP080 PEI (Asia Pacific) ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | |
Sawbones Solid Rigid Polyurethane Foam 5 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Evazote® VA80 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® HD80 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0801 g/cc | 0.00289 lb/in³ | |
Hexcel® HexWeb® HRH-10/F50 - 5.0 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Density | 0.0801 g/cc | 0.00289 lb/in³ | |
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Density | 0.0801 g/cc | 0.00289 lb/in³ | |
Hexcel® HexWeb® HRP - 1/4 - 5.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.0801 g/cc | 0.00289 lb/in³ | |
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core Designation: Material-Cell Size-Density.Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the.. |
|||
Density | 0.0801 g/cc | 0.00289 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 1/8- 5.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | Free Rise Density (Cured) |
Dow BETAFOAM™ 87100/87155 BETAFOAM™ 87100/87155 is a high-density, all-water blown rigid polyurethane foam. These components were engineered to produce a foam for increasing stiffness of body structure cavities. Foam is p.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | Free Rise Density (Cured) |
Dow BETAFOAM™ 87100/87156 BETAFOAM™ 87100/87156 is a rigid, all-water blown molded foam with excellent thermal stability. Foam is produced by rapidly mixing both components under high shear conditions. These components we.. |
|||
Density | 0.0800 - 0.100 g/cc | 0.00289 - 0.00361 lb/in³ | ISO 845-88 |
Eurofoam Evacell EVA 100 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | ISO 845 |
BASF Neopolen® P 9270 0.08 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | ISO 845 |
BASF Neopolen® P 9280 0.08 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |
|||
Density | 0.0801 g/cc | 0.00289 lb/in³ | Free Rise Density, 1% H<sub>2</sub>O |
ACC EP LS EPI Engineered Polymers Leak Stop MDI EP LS, “Powered by Reactamine® Technology”, is a special MDI prepolymer designed to be pumped into voids or walls. EP LS reacts with water to create a shaving cream-like foam. This foam will soli.. |
|||
Density | 0.0800 - 0.120 g/cc | 0.00289 - 0.00434 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Density | 0.0800 - 0.0900 g/cc | 0.00289 - 0.00325 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |
|||
Density | 0.0800 - 0.128 g/cc | 0.00289 - 0.00462 lb/in³ | |
Pyrotek Fiber Seal Y-1 Ceramic fiber paper Y-1 Fiberseal paper is a light-weight refractory material. Y-1 is resistant to most chemicals with the exception of hydrofluoric and phosphoric acids and strong alkalis.ApplicationsGaskets Seals Sp.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | ISO 845 |
BASF Neopolen® P 9255 0.08 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Density | 0.0800 g/cc | 0.00289 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |
|||
Density | 0.0801 g/cc | 0.00289 lb/in³ | |
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Density | 0.0800 - 0.100 g/cc | 0.00289 - 0.00361 lb/in³ | |
Sinotek Materials Soft Graphite Ring Used for electrode joint.Information provided by Sinotek |