Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0960 - 0.128 g/cc | 0.00347 - 0.00462 lb/in³ | |
Pyrotek T-67B Fiberseal Blanket Soluble amorphous wool. Does not contain refractory ceramic fiber.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6, 13, 51 mm thickApplicationsTrough repair Pot bake blanket Flexible joint packaging Carbon.. |
|||
Density | 0.0641 - 0.128 g/cc | 0.00231 - 0.00463 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK1111 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.0641 - 0.128 g/cc | 0.00231 - 0.00463 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK2121 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.0800 - 0.128 g/cc | 0.00289 - 0.00462 lb/in³ | |
Pyrotek Fiber Seal Y-1 Ceramic fiber paper Y-1 Fiberseal paper is a light-weight refractory material. Y-1 is resistant to most chemicals with the exception of hydrofluoric and phosphoric acids and strong alkalis.ApplicationsGaskets Seals Sp.. |