Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.170 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 4.70 g/cc
0.170 lb/in³
ISO 1183
Nilit FRIANYL B63 BR90 Nylon 6.6 for injection molding, 90% bronze filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 4.70 - 5.60 g/cc
0.170 - 0.202 lb/in³
ASTM B417
H.C. Starck Amperit® 558.059 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Density 4.70 - 5.60 g/cc
0.170 - 0.202 lb/in³
ASTM B212
H.C. Starck Amperit® 558.088 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Density 4.70 - 5.60 g/cc
0.170 - 0.202 lb/in³
ASTM B212
H.C. Starck Amperit® 558.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Density 4.70 g/cc
0.170 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR
LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
Density 4.70 g/cc
0.170 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR
LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
Density 4.70 g/cc
0.170 lb/in³
American Elements Molybdenum Oxide Nanopowder
General DescriptionMolybdenum Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles...
Density 4.70 g/cc
0.170 lb/in³
apparent
Wall Colmonoy COLMONOY® 57 PTA - Nickel-Base Hard-Surfacing Alloy
Description: Colmonoy 57 PTA is a unique Ni-Cr-B alloy containing optimized amounts of precipitated tungsten rich hard phases distributed throughout the matrix. These hard phases offer substantial ..
Density 4.70 - 5.60 g/cc
0.170 - 0.202 lb/in³
ASTM B212
H.C. Starck Amperit® 547.002 Tungsten Carbide-Nickel 88-12 (WC-Ni)
Density 4.70 - 5.60 g/cc
0.170 - 0.202 lb/in³
ASTM B417
H.C. Starck Amperit® 547.059 Tungsten Carbide-Nickel 88-12 (WC-Ni)
Density 4.70 - 5.60 g/cc
0.170 - 0.202 lb/in³
ASTM B212
H.C. Starck Amperit® 547.074 Tungsten Carbide-Nickel 88-12 (WC-Ni)
Density 4.70 - 5.60 g/cc
0.170 - 0.202 lb/in³
ASTM B212
H.C. Starck Amperit® 547.088 Tungsten Carbide-Nickel 88-12 (WC-Ni)
Copyright © lookpolymers.com All Rights Reserved