Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wall Colmonoy COLMONOY® 57 PTA - Nickel-Base Hard-Surfacing Alloy

Category Metal , Metal Matrix Composite , Nonferrous Metal , Nickel Alloy
Manufacturer Wall Colmonoy Corporation
Trade Name COLMONOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wall Colmonoy COLMONOY® 57 PTA - Nickel-Base Hard-Surfacing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Colmonoy 57 PTA is a unique Ni-Cr-B alloy containing optimized amounts of precipitated tungsten rich hard phases distributed throughout the matrix. These hard phases offer substantial increase in abrasion resistance and reduce the sensitivity of the material to hardness variations during deposition of overlays using PTA equipment. These hard phases are incorporated in the matrix material by careful alloying during the powder manufacturing process, as opposed to external additions in conventional composite powders. Applications: Colmonoy 57PTA is specifically formulated for overlaying the flights of new and rebuilt extrusion or injection molding screws. It exhibits excellent weldability and is easy for the operator to control. Laboratory tests have shown that variations in PTA deposition parameters have minimal effects on the hardness of the deposit. The alloy also has many other potential applications where resistance to abrasion and corrosion are important. Examples include applications in the food processing industry such as feed screws, air locks and scraper blades. Information provided by Wall Colmonoy Corporation.
Physical Properties Metric English Comments
Density 4.70 g/cc
0.170 lb/in³
apparent
8.50 g/cc
0.307 lb/in³
theoretical
Mechanical Properties Metric English Comments
Hardness, Rockwell C 47
47
single pass
52
52
double pass
Thermal Properties Metric English Comments
Melting Point 971 - 1120 °C
1780 - 2050 °F
Solidus 971 °C
1780 °F
Liquidus 1120 °C
2050 °F
Component Elements Properties Metric English Comments
Boron, B 2.5 %
2.5 %
Carbon, C 0.50 %
0.50 %
Chromium, Cr 11.5 %
11.5 %
Iron, Fe 3.5 %
3.5 %
Nickel, Ni 62.5 %
62.5 %
As Balance
Silicon, Si 3.5 %
3.5 %
Tungsten, W 16 %
16 %