Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.78 g/cc | 0.209 lb/in³ | |
Ferro CF 7578 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific .. |
|||
Density | 5.79 g/cc | 0.209 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 835 Zirconia + 4 mol% Calcia Brand 835 features: High porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal .. |