Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.78 g/cc | 0.209 lb/in³ | |
Ferro CF 7578 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific .. |