Polymer Property : Density = 0.231 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Pacific Sintered Materials F-200-P Iron Powdered Metal
Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-10All information provided by Pacific Sintered Metals.
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI..
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Pacific Sintered Materials FCC-216-P High Carbon Copper Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI..
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Pacific Sintered Materials FCC-216-P(HT) High Carbon Copper Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI..
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Pacific Sintered Materials FCC-221-P Copper Steel Powdered Metal
Applications:Medium strength mechanical componentsEquivalent MPIF Specification: FC-0205-35All information provided by Pacific Sintered Metals.
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
PSM Industries Pacific Sintered Metals Copper Steel FC-221-P Powdered Metal
Medium strength mechanical components Equivalent MPIF Specification: FC-0205-35Information Provided by Pacific Sintered Metals, a division of PSM Industries
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-200-P Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP..
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP..
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P(HT) Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP..
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
PSM Industries Pacific Sintered Metals Iron F-200-P Powdered Metal
Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-10Information Provided by Pacific Sintered Metals, a division of PSM Industries