Polymer Property : Density = 0.265 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 7.34 g/cc
0.265 lb/in³
Indium Corp. Indalloy 123 Tin Solder Alloy
Information Provided by Indium Corporation
Density 7.34 g/cc
0.265 lb/in³
Williams Advanced Alloys WS226A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 7.34 g/cc
0.265 lb/in³
ATI Allegheny Ludlum ALFA-II™ Stainless Steel Type 406
Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat..