Williams Advanced Alloys WS226A Solder

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS226A Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 7.34 g/cc
0.265 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.7 MPa
6200 psi
Thermal Properties Metric English Comments
CTE, linear 19.5 µm/m-°C

@Temperature 20.0 °C
10.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Melting Point 221 - 226 °C
430 - 439 °F
Solidus 221 °C
430 °F
Liquidus 226 °C
439 °F
Component Elements Properties Metric English Comments
Silver, Ag 2.5 %
2.5 %
Tin, Sn 97.5 %
97.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001536 ohm-cm
0.00001536 ohm-cm