Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.37 g/cc | 0.266 lb/in³ | |
Indium Corp. Indalloy 251 Tin Solder Alloy Castin Patented alloyInformation Provided by Indium Corporation |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | |
Indium Corp. Indalloy® 121 Sn-Ag Solder Alloy Binary solder has history of use, marginal wetting. Standard tin-silver eutectic solder with wide application when lead-based solders do not meet temperature, strength or safety requirements. Not r.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | |
Indium Corp. Indalloy® 231 Sn-Zn-In-Bi Solder Alloy Pb free solder. Zn causes high drossing; corrosion concerns.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.37 g/cc | 0.266 lb/in³ | |
Indium Corp. Indalloy® 254 86.9Sn/10.0In/3.1Ag Lead-Free Solder Alloy No Sn/In eutectic problem; potential use for flip chip assembly. Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | |
Lucas-Milhaupt Silvabrite® 100® Lead-Free Solder Silvabrite 100® was developed to meet market demands for a safe and easy to use solder for drinking water systems and other applications. Silvabrite 100® is a lead-free and antimony-free, non-.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | Weld Deposit Property |
The NanoSteel® Company SHS 9700 GMAW OAW Steel Alloy, Cored Wire Coating Description: SHS 9700 GMAW OAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that features exceptional abrasive wear resistance with superior toughness and no.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | Weld Deposit Property |
The NanoSteel® Company SHS 9700 PTAW Steel Alloy, Atomized Powder Coating Description: SHS 9700 PTAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that features good abrasion and fine particle erosion resistance with no high-cost ni.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | Deposit Property |
The NanoSteel® Company SHS 9700 Steel Alloy, Wear Plate Coating Description: SHS 9700 wear plate has been designed to outperform carbide overlays and quench & temper steel wear plate, such as Brinell, AR-steel and Hardox.Key Performance Characteristics66.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | Weld Deposit Property |
The NanoSteel® Company SHS 9700E Steel Alloy, Stick Electrode Coating Description: SHS 9700E Stick Electrode is an iron based steel alloy with a near nanoscale (submicron) microstructure that features exceptional abrasive wear resistance with superior toughnes.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | Weld Deposit Property |
The NanoSteel® Company SHS 9800 GMAW OAW Steel Alloy, Cored Wire Coating Description: SHS 9800 GMAW OAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that includes chromium, molybdenum and niobium in the material chemistry, resulti.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | Deposit Property |
The NanoSteel® Company SHS 9800 Steel Alloy, Wear Plate Coating Description: SHS 9800 is a patented iron based glass forming steel alloy with a near nanoscale (submicron) microstructure that includes chromium, molybdenum and niobium in the material chemi.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | |
Williams Advanced Alloys WS221 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.37 g/cc | 0.266 lb/in³ | |
Williams Advanced Alloys WS226 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | |
Trimay® Wear Plate T171 Iron-based Steel Overlay Overlay Description: T171 is a patented iron based steel overlay wear solution with a near nanoscale (submicron) microstructure. T171 is well suited for the toughest jobs in the most extreme service.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | |
Trimay® Wear Plate TWP171 Iron-based Steel Alloy Weld Wire Overlay Description: TWP171w GMAW OAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that includes chromium, molybdenum and niobium in the material chemistry, resultin.. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | |
AIM 95Sn/3.5Ag/1.5In Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 7.36 g/cc | 0.266 lb/in³ | |
AIM 96.5Sn/3.5Ag Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |