Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.756 g/cc | 0.2802 lb/in³ | |
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |
|||
Density | 7.756 g/cc | 0.2802 lb/in³ | |
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Transverse Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |
|||
Density | 7.756 g/cc | 0.2802 lb/in³ | |
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Longitudinal Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |
|||
Density | 7.756 g/cc | 0.2802 lb/in³ | |
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Transverse Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |