Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 7.756 g/cc
0.2802 lb/in³
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Density 7.756 g/cc
0.2802 lb/in³
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Transverse Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Density 7.756 g/cc
0.2802 lb/in³
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Longitudinal Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Density 7.756 g/cc
0.2802 lb/in³
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Transverse Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..