Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Latrobe LSSâ„¢ 17-4 Precipitation Hardening Stainless Steel (ASTM Type 360) TLS 17-4 is a precipitation hardening, martensitic stainless steel that exhibits excellent resistance to atmospheric and chemical corrosion. TLS 17-4 exhibits an excellent combination of high stren.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
International Mold Steel DHA-World Die Cast & Forging Steel DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Weartech International WT-60 Nickel Hardfacing & Wear Resistant Alloy Applications: pump sleevesInformation provided by Weartech International |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Crucible Steel Cru-Wear® Tool Steel CRU-WEAR is an air-hardening tool steel, heat treatable to HRC 60-65. Designed as an upgrade to D2, it offers better wear resistance, greater toughness and higher attainable hardness. Compared to th.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Crucible Steel MAXEL® 3-1/2 (Brake Die) Free-Machining Alloy Steel, AISI 4150 S MAXEL 3-1/2 free-machining alloy steel provides a good combination of heat treated properties and machinability. This alloy steel is manufactured under close quality control to an ASTM grain size of.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | hardened to 57 HRC |
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 925 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | Typical |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1025 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | Typical |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type AL 436S™ Ferric Stainless Steel The AL 436S™ alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Angular titanium carbo-nitiride particles occur randomly in the ferrite matrix mi.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
ATI Allvac® Vasco® 15-5 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age Data provided by Allvac.Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1075 (Heated 579°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Assab Steels 718HH Plastic Mold Material IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34 Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Latrobe Dynamax™ ASTM M42, DIN 1.3247 Super High Speed Steel Dynamax super high speed steel is a premium cobalt high speed steel with a chemical composition designed for high hardness and superior hot hardness. These properties make the steel an excellent cho.. |