Polymer Property : Density = 0.295 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.17 g/cc
0.295 lb/in³
IBC Advanced Alloys 42C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
Density 8.17 g/cc
0.295 lb/in³
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel
CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge..
Density 8.17 g/cc
0.295 lb/in³
theoretical
Kennametal Stellite Deloro® 716 PM cast
Adhesive wear test data: cast 0.1; abrasive wear test data: cast 63 mm^3. Deloro 716 is currently being developed. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball ..
Density 8.17 g/cc
0.295 lb/in³
theoretical
Kennametal Stellite Deloro® 716 PM with P/M Processing
Adhesive wear test data: cast 0.1; abrasive wear test data: cast 63 mm^3. Deloro 716 is currently being developed. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball ..
Density 8.16 g/cc
0.295 lb/in³
Indium Corp. Indalloy 108 Tin-Lead Solder Alloy
Good pre-tinning alloyInformation Provided by Indium Corporation
Density 8.17 g/cc
0.295 lb/in³
Latrobe Corsairâ„¢ ASTM M3-1 High Speed Steel
CORSAIR (M3-1) contains carbon and vanadium levels that are intermediate between those of Double Six (M2) and Crusader (M3-2). This gives the steel a fine balance of wear resistance and grindability..
Density 8.17 g/cc
0.295 lb/in³
Special Metals INCOLOY® alloy 908
INCOLOY® alloy 908 (UNS N09908) is an age-hardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue cr..
Density 8.16 g/cc
0.295 lb/in³
Special Metals NILO® Alloy K Controlled-Expansion Alloy
Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat..
Density 8.17 g/cc
0.295 lb/in³
Williams Advanced Alloys WS186 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 8.17 g/cc
0.295 lb/in³
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel
CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea..
Density 8.17 g/cc
0.295 lb/in³
Crucible Steel REX® M3-1 High Speed Steel, AISI M3-1
REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results in better machining and grinding characteristics compared to M3-2, with a slight im..
Density 8.17 g/cc
0.295 lb/in³
California Fine Wire Manganin 230 (Shunt) Copper, Manganese, and Nickel Resistance Wire
All values may vary dependent on specific design and usageNickel content modifiedCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Density 8.16 g/cc
0.295 lb/in³
ATI Allvac® Nickelvac® 80 A UNS N07080 Nickel Superalloy
Uses: Components for gas turbine engines, exhaust valve stock for internal combustion engines, high temperature bolts & fasteners.Property values are for samples in the metallurgical condition: 1700..
Density 8.17 g/cc
0.295 lb/in³
ATI Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000
The alloy produces good magnetic properties, wide latitude to control hysteresis loop shape via recrystallization modes. Applications for this grade range from electromechanical relay cores, to ver..