Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.16 g/cc | 0.295 lb/in³ | |
Indium Corp. Indalloy 108 Tin-Lead Solder Alloy Good pre-tinning alloyInformation Provided by Indium Corporation |
|||
Density | 8.16 g/cc | 0.295 lb/in³ | |
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
Density | 8.16 g/cc | 0.295 lb/in³ | |
ATI Allvac® Nickelvac® 80 A UNS N07080 Nickel Superalloy Uses: Components for gas turbine engines, exhaust valve stock for internal combustion engines, high temperature bolts & fasteners.Property values are for samples in the metallurgical condition: 1700.. |