Density 8.20 - 8.30 g/cc
0.296 - 0.300 lb/in³
Kennametal Stellite Denertiaâ„¢ N8 Nickel Dental Alloy
Denertiaâ„¢ N8 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium free as defined by ISO 22674Information pr..