Physical Properties Metric English Comments
Density 11.02 g/cc
0.3981 lb/in³
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy
Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation.
Density 11.02 g/cc
0.3981 lb/in³
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy
This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm..
Density 11.02 g/cc
0.3981 lb/in³
Williams Advanced Alloys WS296 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 11.02 g/cc
0.3981 lb/in³
Williams Advanced Alloys WS300 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys