Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 11.02 g/cc
0.3981 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.1 MPa
3500 psi
Thermal Properties Metric English Comments
CTE, linear 24.0 µm/m-°C

@Temperature 20.0 °C
13.3 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 26.0 W/m-K
180 BTU-in/hr-ft²-°F
Melting Point 287 - 296 °C
549 - 565 °F
Solidus 287 °C
549 °F
Liquidus 296 °C
565 °F
Component Elements Properties Metric English Comments
Lead, Pb 92.5 %
92.5 %
Silver, Ag 2.5 %
2.5 %
Tin, Sn 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00002263 ohm-cm
0.00002263 ohm-cm
Users viewing this material also viewed the following: