Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 14.0 g/cc | >= 0.506 lb/in³ | |
Hogen Duralloy H5W 70 Tungsten/30 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
Density | >= 14.0 g/cc | >= 0.506 lb/in³ | |
Mi-Tech Metals CW70 70 Tungsten/30 Copper PM Metal Composite RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme.. |
|||
Density | 14.0 g/cc | 0.506 lb/in³ | |
Wieland 1403 Wilaform Gold Hard yellow gold alloy. Universally applicable in decoration production. Since it does not posses a very fine-grained structure it is used frequently for chainsApplications: casting, chains, lamin.. |
|||
Density | 14.0 - 14.5 g/cc | 0.506 - 0.524 lb/in³ | |
China Tungsten YG11C Cemented Tungsten Carbide for Mining Purposes For tipping of bits for heavy rock drills and rotary hammer rock drills cutting hard rock formations . e. g. , latent hole drills and deep-hole drills, rock drills, etc.Information provided by China.. |
|||
Density | 14.0 - 14.3 g/cc | 0.506 - 0.517 lb/in³ | |
China Tungsten YG13C Cemented Tungsten Carbide for Mining Purposes For oil cone drills, for hard and medium hard rock and for tipping bit of rotary hammer rock drills and heavy rock drills.Information provided by China Tungsten |
|||
Density | 14.0 g/cc | 0.506 lb/in³ | |
China Tungsten YG15 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Density | 14.0 g/cc | 0.506 lb/in³ | |
China Tungsten YG15C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Density | 14.0 g/cc | 0.506 lb/in³ | |
China Tungsten YG15X Tungsten Carbide Powder Information provided by China Tungsten |