Polymer Property : Density = 0.517 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 14.0 - 14.3 g/cc
0.506 - 0.517 lb/in³
China Tungsten YG13C Cemented Tungsten Carbide for Mining Purposes
For oil cone drills, for hard and medium hard rock and for tipping bit of rotary hammer rock drills and heavy rock drills.Information provided by China Tungsten