Physical Properties Metric English Comments
Density 14.4 - 14.7 g/cc
0.520 - 0.531 lb/in³
China Tungsten K05 Tungsten Carbide for Mining Purposes
High toughness, wear resistance and performance, for single line and cross bits of rotary hammer rock drills for hard rock formations.Information provided by China Tungsten
Density 13.5 - 14.7 g/cc
0.488 - 0.531 lb/in³
China Tungsten YT6S Tungsten Carbide
Having the same wear resistance as YG6X but higher toughness. for tobacco cutters and rough and finish milling of cast iron.Information provided by China Tungsten