Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.4 - 14.7 g/cc | 0.520 - 0.531 lb/in³ | |
China Tungsten K05 Tungsten Carbide for Mining Purposes High toughness, wear resistance and performance, for single line and cross bits of rotary hammer rock drills for hard rock formations.Information provided by China Tungsten |
|||
Density | 13.5 - 14.7 g/cc | 0.488 - 0.531 lb/in³ | |
China Tungsten YT6S Tungsten Carbide Having the same wear resistance as YG6X but higher toughness. for tobacco cutters and rough and finish milling of cast iron.Information provided by China Tungsten |