Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 18.5 g/cc
0.668 lb/in³
Hogen HM3750 Tungsten-Based Metal
Mil Spec T-21014D Class 4; ASTM B-777-99 Class 4; AMS T-21014 Class 4. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE..
Density 18.5 g/cc
0.668 lb/in³
MarkeTech 97-2-1 Tungsten Alloy, AMS-T-21014 Class 4
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Density 18.5 g/cc
0.668 lb/in³
Mi-Tech Metals HD18.5 Tungsten-Based Metal
Mil Spec T-21014D Class 4; ASTM B-777-99 Class 4; ASTM B-777-07 Class 4; AMS T-21014 Class 4. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con..
Density 18.5 g/cc
0.668 lb/in³
Wieland Porta AB 76 Casting Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, ceramic veneering, acrylic veneeringDental
Density 18.5 g/cc
0.668 lb/in³
Wieland Porta Geo Ti PFM Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental
Density 18.5 g/cc
0.668 lb/in³
CMW® 3970 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, OrdnanceInformation provided by CMW Inc.