Wieland Porta AB 76 Casting Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Platinum Alloy
Manufacturer Wieland
Trade Name Porta
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Porta AB 76 Casting Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, ceramic veneering, acrylic veneeringDental
Physical Properties Metric English Comments
Density 18.5 g/cc
0.668 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 160
160
HV5/30; after porcelain firing
190
190
HV5/30; hardened
Tensile Strength, Yield 400.00 MPa

@Strain 0.200 %
58015 psi

@Strain 0.200 %
after porcelain firing
510.00 MPa

@Strain 0.200 %
73969 psi

@Strain 0.200 %
hardened
Elongation at Break 5.0 %
5.0 %
hardened
10 %
10 %
after porcelain firing
Modulus of Elasticity 102 GPa
14800 ksi
Thermal Properties Metric English Comments
CTE, linear 14.3 µm/m-°C

@Temperature 25.0 - 500 °C
7.94 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Copper, Cu 0.40 %
0.40 %
Gold, Au 84.5 %
84.5 %
Indium, In 1.0 %
1.0 %
Iridium, Ir 0.10 %
0.10 %
Iron, Fe 0.20 %
0.20 %
Palladium, Pd 4.5 %
4.5 %
Platinum, Pt 8.3 %
8.3 %
Silver, Ag 0.50 %
0.50 %
Tin, Sn 0.50 %
0.50 %
Processing Properties Metric English Comments
Processing Temperature 799 °C
1470 °F
Preheating Temp.
Melt Temperature 1060 - 1180 °C
1940 - 2160 °F
Casting Temperature 1330 °C
2430 °F
Descriptive Properties Value Comments
Color pale yellow