Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 19.3 g/cc | 0.697 lb/in³ | |
Indium Corp. Indalloy 200 Pure Gold Information Provided by Indium Corporation |
|||
Density | 19.3 g/cc | 0.697 lb/in³ | |
Wieland 1964 Wilaform Gold Fine gold. Universally applicable for sheet metals, volumes, pipes, profiles and contacts.Applications: chains, coin/shape, pipesDental |
|||
Density | 19.3 g/cc | 0.697 lb/in³ | |
CMW® ELKON 100W Pure Tungsten Tungsten, also called Wolfram, occurs as an impure tungsten oxide in wolframite and sche ores. It is chemically extracted, refined to an oxide of high purity and reduced to tungsten powder in hydrog.. |