Wieland 1964 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Pure Element
Manufacturer Wieland
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1964 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fine gold. Universally applicable for sheet metals, volumes, pipes, profiles and contacts.Applications: chains, coin/shape, pipesDental
Physical Properties Metric English Comments
Density 19.3 g/cc
0.697 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 25
25
HV5; glowed
Tensile Strength, Ultimate 125 MPa
18100 psi
Elongation at Break 30 %
30 %
Thermal Properties Metric English Comments
Melting Point 1064 °C
1947 °F
Component Elements Properties Metric English Comments
Gold, Au 99.9 %
99.9 %
Other 0.010 %
0.010 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1120 - 1260 °C
2050 - 2300 °F
Descriptive Properties Value Comments
Color full-yellow