Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.800 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres
EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t..
Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ CG Hollow Spheres
EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t..
Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ FM-1 Hollow Spheres
EXTENDOSPHERESâ„¢FM-1 ceramic hollow spheres are a low-density functional additive for disc brake pads, truck and train blocks, clutch facings and other friction materials. They are compatible wi..
Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ HA Hollow Spheres
EXTENDOSPHERESâ„¢ HA are off white, low-cost, low-density, high alumina, ceramic hollow spheres.Applications: Hollow spheres are ideal for use in coatings, sealants, caulks and other applications..
Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ MG Hollow Spheres
EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t..
Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ SG Hollow Spheres
EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t..
Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ TG Hollow Spheres
EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t..
Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 CM-OPC EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.0180 - 0.800 g/cc
0.000650 - 0.0289 lb/in³
BASF Styropor® BFL 327 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c..
Copyright © lookpolymers.com All Rights Reserved