Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.700 g/cc | 0.0253 lb/in³ | Average Density |
Potters Industries Conduct-O-Fil® AGSF-20 Silver-coated Hollow Ceramic Spheres Applications: Conductive paints and coatings; Aerospace and other mass-critical applications. Advantages include low density, easily mixed into paint systems, large particle sizeInformation provide.. |
|||
Density | 0.700 - 1.20 g/cc | 0.0253 - 0.0434 lb/in³ | Average value: 1.17 g/cc Grade Count:249 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Density | 0.700 - 1.56 g/cc | 0.0253 - 0.0564 lb/in³ | Average value: 1.43 g/cc Grade Count:19 |
Overview of materials for Chlorinated PVC (CPVC) This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.700 - 3.80 g/cc | 0.0253 - 0.137 lb/in³ | Average value: 1.31 g/cc Grade Count:923 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Density | >= 0.700 g/cc @Temperature 20.0 °C |
>= 0.0253 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-15 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | ISO 1183 |
Lucobit Lucowax® 1700 Polyethylene Wax Lucowax is a polyethylene wax additive for the modification of bitumen or asphalt.The addition of Lucowax reduces viscosity and penetration, while increasing water resistance, plasticity, and deform.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | |
Synergy Polymers Ultra Purge HT Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | |
Synergy Polymers Ultra Purge LOW-E Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | |
Synergy Polymers Ultra Purge Plus Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents. Moldable compou.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | |
Synergy Polymers Ultra Purge P-O Ultra Purge is a specially designed cleaning compound that comes premixed and ready-to-use in pellet form. It cleans black specks and deposits from screws, barrels, nozzle, hot runners and heads of .. |
|||
Density | <= 0.700 g/cc @Temperature 0.850 °C |
<= 0.0253 lb/in³ @Temperature 33.5 °F |
|
Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - .. |
|||
Density | <= 0.700 g/cc @Temperature 0.850 °C |
<= 0.0253 lb/in³ @Temperature 33.5 °F |
|
Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride >94% CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - .. |
|||
Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Shandong Dongyue Polymer DF-31A PTFE Pelletized Resin Usage: The resin is used to auto press molding and ram extrusion all kinds of rods, pipe etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ FM-1 Hollow Spheres EXTENDOSPHERESâ„¢FM-1 ceramic hollow spheres are a low-density functional additive for disc brake pads, truck and train blocks, clutch facings and other friction materials. They are compatible wi.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ HA Hollow Spheres EXTENDOSPHERESâ„¢ HA are off white, low-cost, low-density, high alumina, ceramic hollow spheres.Applications: Hollow spheres are ideal for use in coatings, sealants, caulks and other applications.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ MG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ TG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials B Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials B Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.07 |
Sinotek Materials D Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 1183 |
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulatio.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | Apparent; ASTM D1182 |
Chi Mei Acryrex® CM-205 PMMA High heat injection grade. It can resist high temperature. High mechanical strength.Applications: The indicator cover of scooter and automobile/sun glasses/digital watch cover.Features:Good Weather .. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | |
Arkema Group Lucalor® RB 8067 CPVC, Pipe Grade LUCALOR RB 8067 is the trade name for CPVC made by Elf Atochem. It is manufactured with a patented mass PVC resin chlorination process.* MAIN CHARACTERISTICS Chlorine content:67.0%. Viscosity index .. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM C134 |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials A Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials A Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.06 |
Sinotek Materials C Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.06 |
Sinotek Materials C Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.07 |
Sinotek Materials D Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |