Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 51-35BP HDPE Extrusion Resin Features: Medium molecular weight, excellent ESCR, excellent toughness, good processability, good chemical resistance.Applications: Extrusion on to metal pipes to produce a corrosion resistant coati.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Reliance Industries Relene S42005 Polyethylene Wire and cable High Density Polyethylene grade. Characteristics: excellent processing, superior physical/electrical properties, good environmental stress crack resistance. Applications: recommended .. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2405 20% Ethylene-Methyl Acrylate Copolymer
(discontinued **) Westlake EMAC® SP2405 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperature are required. SP2405 provides.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil LL 3402.48 Cast Film Resin
(discontinued **) LL 3402.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex.. |
|||
Density | 0.942 - 0.946 g/cc | 0.0340 - 0.0342 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6844G (446H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Chevron Phillips mPact™ D449 HDPE Blown Film Resin
(discontinued **) Resin Type: High density, hexene copolymerCharacteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer.Applications: overw.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | Base Density |
NOVA Chemicals Sclair® 35BP HDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-721 High EVA Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity.App.. |
|||
Density | 0.942 - 0.949 g/cc | 0.0340 - 0.0343 lb/in³ | Average value: 0.946 g/cc Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade ALATHON H4250 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) HB4265 High Density Polyethylene HB4265 is a high molecular weight high density polyethylene.Applications: tanks, industrial, blow molding.Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/2-LR UV Polyolefin Catalyst CT/2-LR UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds,.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | Base; ASTM D792 |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Westlake EMAC® Plus SP1305 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1305 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1305 is.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D4883 |
Westlake Tymax™ GA7001 Anhydride Modified Acrylate Copolymer (Developmental) Westlake GA7001 is an anhydride modified acrylate copolymer for extrusion coating and cast film tie-layers. This resin is designed to function as a coextruded tie-layer in multilayer applications. W.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00119 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene blown film grade for applications requiring high stiffness. It can also be used in cast films. Films produced from the resin e.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 3404.48 Linear Low Density Polyethylene Resin Product Description: LL 3404.48 is a hexane medium density polyethylene cast film grade for applications requiring high strength and high stiffness. Films produced from this resin exhibit good tensi.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | Exxon Method |
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer. TC 110 can be used for injection molding applications. It can be used in alloys, blends or compounds to increase impact s.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D4883 |
ExxonMobil HD 8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D4883 |
ExxonMobil HDP8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM-D792 |
Braskem FH35 HDPE Cast Film Extrusion Polyethylene Copolymer The FH35 resin is a high-density polyethylene, copolymer of butene-1, produced by the solution process for flat die film extrusion with good mechanical properties. It contains antioxidant additives... |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® HD-8660 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® HD-8661 HDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | Exxon Method |
ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formula.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | Exxon Method |
ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formula.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil ESCOR™ AT 310 Molding, extrusion and compounding resin
(discontinued **) ESCOR AT 310 provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable for use as a polymer modifier .. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | Base Resin; ASTM D792 |
Borealis Borstar® HE6063 Natural Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6063 is a natural, colorable, bimodal, high-density polyethylene compound, produced using the Borstar process, for jacketing of power and telecommunications cables. It is characterized by.. |