Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.963 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
Network Polymers NPP 50-0863
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
SABIC CC862 High Density Polyethylene for Injection Molding
Product Description: SABIC HDPE CC862 is a high density polyethylene specially developed for still water bottle caps that meet organoleptic properties requirements. The material offers and ideal c..
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
Huntsman Rexell® H2105 Injection Molding LLDPE  (discontinued **)
Linear-low high density, injection molding, FDA compliant.Features: High impact strength with reasonable flow.Applications: Articles that must withstand long-term heavy loading such as bottle crates..
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
Chevron Phillips HiD® 9402 HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Homopolymer; Blow Molding, Sheeting and Profile ResinCharacteristics: High Melt Strength - Larger Parts, Wide Range of Processing Conditions, High Stiffness and Impact Resistance,..
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
Chevron Phillips Marlex® HHM TR-166 Polyethylene, Film Grade; HDPE  (discontinued **)
FDA approved.Data provided by the manufacturer
Density 0.963 g/cc
0.0348 lb/in³
ISO 1183
Total Finathene® 6006 HDPE, blow molding, pipe  (discontinued **)
Finathene® 6006 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Polymerization is conducted in the absence of any other comonomer. Finathene® 6006 h..
Density 0.963 g/cc
0.0348 lb/in³
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade
Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats..
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
Ineos A60-70-162 HDPE
Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character..
Density 0.963 g/cc
0.0348 lb/in³
ISO 1183
Borealis BL2631 High Density Polyethylene
BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi..
Density 0.963 g/cc
0.0348 lb/in³
ISO 1872-2/ISO 1183
Borealis Borcell™ HE1123 High Density Polyethylene
Borcell™ HE1123 is a high density polyethylene compound intended for the insulation of radio frequency coaxial cables. Borcell™ HE1123 is designed to give the lowest possible cable attenuation by..
Density 0.963 g/cc
0.0348 lb/in³
ISO 1183
Unipetrol PE HD LITEN® MB/ML 72 HDPE
Made for injection molding applications.Information provided by Unipetrol RPA
Density 0.963 g/cc
0.0348 lb/in³
ISO 1183
Unipetrol PE HD LITEN® MB/ML 73 HDPE
Made for injection molding applications.Information provided by Unipetrol RPA
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ExxonMobil HDPE AP60-007 High Density Polyethylene Resin
Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ExxonMobil Paxon™ AA60-003 Blow Molding Resin
Product Description: AA60-003 is a medium molecular weight distribution high density polyethylene which is characterized by high stiffness, excellent melt uniformity, and chemical inertness.Availabi..
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ExxonMobil Paxon™ AD60-005 Blow Molding Resin
Product Description: AD60-005 is a medium molecular weight districution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ExxonMobil Paxon™ AD60-007 Blow Molding Resin
Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
Density 0.963 g/cc
0.0348 lb/in³
Dow HDPE 05862N High Density Polyethylene
Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
Density 0.963 g/cc
0.0348 lb/in³
ASTM D-792
Bapolene® 3257U Polyethylene, Injection Molding
Bapolene 3257U is a high density polyethylene resin that offers improved cycle times, superior modulus and impact resistance. It complies with US FDA 21CFR177.1520 and has a UV protection package.A..
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ExxonMobil Paxon™ 4700 Blown Film Extrusion Resin  (discontinued **)
4700 is a medium molecular weight, high density polyethylene homopolymer film resin. It can be processed on conventional film extrusion equipment.Information provided by ExxonMobil Chemical
Density 0.963 g/cc
0.0348 lb/in³
ISO 1183
Unipetrol PE HD LITEN® MB/ML 71 HDPE
Made for injection molding applications.Information provided by Unipetrol RPA
Copyright © lookpolymers.com All Rights Reserved