Bapolene® 3257U Polyethylene, Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 3257U Polyethylene, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene 3257U is a high density polyethylene resin that offers improved cycle times, superior modulus and impact resistance. It complies with US FDA 21CFR177.1520 and has a UV protection package.Applications: Pallets, crates, and pails.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D-792
Melt Flow 10 g/10 min
10 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A <=
<=
ASTM D-2240
Tensile Strength, Yield 26.30 MPa
3815 psi
ASTM D-638
Elongation at Break 1175 %
1175 %
ASTM D-638
Flexural Modulus 1.29 GPa
187 ksi
ASTM D-790
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution