Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.999 g/cc | 0.0361 lb/in³ | ISO 1183 |
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed.. |