Polymer Property : Density = 1.234 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.234 g/cc
0.04458 lb/in³
Dow PAPI™ 94 Polymeric MDI
PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This products low viscosity, low functionality, increased diphenylmethane diisocyanate content and increased perc..
Density 1.234 g/cc
0.04458 lb/in³
Dow PAPI™ 95 Polymeric MDI
PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethan..
Density 1.234 g/cc
0.04458 lb/in³
Dow PAPI™ 20 Polymeric MDI
PAPI™ 20 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality value of 3.2 and high viscosity result in highly rigid foams. This product is design..
Density 1.234 g/cc
0.04458 lb/in³
ISO 1183
BASF Ultrason® S 3010 MR UN PSU
Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1..