Physical Properties Metric English Comments
Density 1.241 g/cc
0.04485 lb/in³
Blue River Coatings Undercoat Primer
BLUE RIVER COATINGS UNDERCOAT PRIMER is a high quality, single component primer, not requiring any catalyzing agent. Performance obtained is equal or superior to that of two-component, catalyzed epo..
Density 1.241 g/cc
0.04485 lb/in³
Blue River Coatings Low VOC Primer Sealer
BLUE RIVER COATINGS LOW VOC PRIMER SEALER is a high quality, single component primer. Performance obtained is equal or superior to that of single component solvent primers. LOW VOC PRIMER SEALER off..
Density 1.241 g/cc
0.04485 lb/in³
Blue River Coatings Primer Sealer-PSWP
BLUE RIVER COATINGS PRIMER SEALER-PSWP is a high quality, single component primer formulated specifically for priming wood, vinyl, and most plastic substrates. Performance obtained is equal or super..
Density 1.241 g/cc
0.04485 lb/in³
Blue River Coatings Wood Primer
BLUE RIVER COATINGGS WOOD PRIMER is a high quality, single component primer, not requiring any catalyzing agent. WOOD PRIMER offers good coverage, excellent durability, and ease of application, as w..