Material Notes:
BLUE RIVER COATINGS UNDERCOAT PRIMER is a high quality, single component primer, not requiring any catalyzing agent. Performance obtained is equal or superior to that of two-component, catalyzed epoxy systems. UNDERCOAT PRIMER offers good coverage, excellent durability, and ease of application, as well as being a low VOC and EPA compliant coating. Enviromental Advantages:BLUE RIVER COATINGS UNDERCOAT PRIMER is a low VOC (Volatile Organic Compound), high performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.Characteristics: Excellent exterior durabilityExcellent hardness/impact resistanceExcellent mar and abrasion resistanceExcellent adhesion on plastics and gel coat substratesSolvent resistantCan be applied in a wide variety of temperature and humidity conditions without the use of retardersDistilled water is used for reductionWater is used for clean-upNon-HazardousAir dry or force curing preferredCan be oven bakedWide range of colorsCoating will not flash rust on bare metalShelf life of 1 yearUnused paint can be returned to containerNon-FlammableUsesSteelAluminumFiberglassConcretePlasticsPVCTruck chassis Automobile chassisTrailersHeavy equipmentSalt Fog in Harshaw No. 22 cabinet via ASTM B117 procedures with 5% NaCl solution. Evaluation of panels follows ASTM D610, D714, and D1654.1512 hoursScribed – 1/16” dense #4. Moderate rust rundown OK – moderate rust rundownUnscribed – OK – moderate rust rundownTested by McWhorter TechnologiesInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Density 1.241 g/cc
0.04485 lb/in³
Solids Content 40.62 %
40.62 %
by volume
43.2 %
43.2 %
by weight
Volatile Organic Compounds (VOC) Content 240 g/l
240 g/l
pH 7.0 - 8.5
7.0 - 8.5
Mechanical Properties Metric English Comments
Impact Test 20.3 J
15.0 ft-lb
Reverse on steel
Thermal Properties Metric English Comments
Boiling Point 169 °C
336 °F
Flash Point 65.6 °C
150 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Dust Free, at 50% humidity
19.8 min

@Temperature 75.0 °C
0.330 hour

@Temperature 167 °F
Recoat, at 50% humidity
30.0 min

@Temperature 75.0 °C
0.500 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesion Excellent; Steel, Plastic, and Aluminum.
Evaporation Rate Slower than ether
Theoretical Coverage 652 ft2 at 1 mil
Vapor Density Heavier than air