Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.276 g/cc @Temperature 70.0 °C |
0.04610 lb/in³ @Temperature 158 °F |
|
Solvay Chemicals Glycerol alpha monochlorohydrin Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay |
|||
Density | 1.276 g/cc | 0.04610 lb/in³ | |
Solvay Chemicals DIGLYCEROL Diglycerol is a clear viscous liquid very similar to glycerol. It has a higher molecular weight than glycerol and is less volatile. It is water soluble and can be combined with aqueous systems.EINEC.. |