Solvay Chemicals DIGLYCEROL

Category Fluid
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals DIGLYCEROL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Diglycerol is a clear viscous liquid very similar to glycerol. It has a higher molecular weight than glycerol and is less volatile. It is water soluble and can be combined with aqueous systems.EINECS Number: 261-605-5/CAS Number: 59113-36-9Information provided by Solvay
Physical Properties Metric English Comments
Density 1.276 g/cc
0.04610 lb/in³
Viscosity 13000 cP
13000 cP
Dynamic
Thermal Properties Metric English Comments
CTE, linear 530 µm/m-°C

@Temperature 20.0 - 60.0 °C
294 µin/in-°F

@Temperature 68.0 - 140 °F
Specific Heat Capacity 2.28 J/g-°C
0.545 BTU/lb-°F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
Boiling Point 205 °C

@Pressure 0.000130 MPa
401 °F

@Pressure 0.0189 psi
Flash Point 230 °C
446 °F
Optical Properties Metric English Comments
Refractive Index 1.487
1.487
Electrical Properties Metric English Comments
Dielectric Constant 34
34
Descriptive Properties Value Comments
Autoignition 380°C
Color <30
APHA
Composition <0.5 g/kg
Water
<50 mg/kg
Chloride
>90%
Diglycerol
Fire point 264°C
Heat of dissolution in water -52 j/g