Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.289 g/cc | 0.04657 lb/in³ | ASTM D1505 |
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating Parylene C is a polymer of para-xylylene modified by the substitution of a chlorine atom for one of the aromatic hydrogen atoms. Parylene C has a useful combination of electrical and physical proper.. |
|||
Density | 1.289 g/cc | 0.04657 lb/in³ | Melt; ISO 1183 |
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The com.. |
|||
Density | 1.289 g/cc | 0.04657 lb/in³ | |
Parylene Coating Services C Poly (P-Xylylene) Monomer is monochloro para-xylylene. Parylene C is recommended where excellent barrier protection is needed. It can be used up to 125°C where oxygen is present.Parylene is a generic name for poly-.. |