Polymer Property : Density = 1.602 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.602 g/cc
0.05788 lb/in³
Pyrotek NAD-250 Structural Insulation Board
NAD-250 is a general purpose cement board. It is suitable for low-voltage electrical insulation in dry conditions.ApplicationsOven shelves Platen insulators Coil boxes Foundry core plates Heat guar..
Density 1.602 g/cc
0.05788 lb/in³
Pyrotek TS-330 Thermoset Electrical Insulation Product
Glass reinforcement, Polyester resin, Light Orange color. Very high compressive and flexural strength.Information provided by Pyrotek.