Pyrotek NAD-250 Structural Insulation Board

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek NAD-250 Structural Insulation Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NAD-250 is a general purpose cement board. It is suitable for low-voltage electrical insulation in dry conditions.ApplicationsOven shelves Platen insulators Coil boxes Foundry core plates Heat guards AdvantagesHigh strength Thermal stability Corrosion resistance Flame resistance Good machinability Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.602 g/cc
0.05788 lb/in³
Water Absorption 21 %
21 %
Mechanical Properties Metric English Comments
Flexural Strength 18.0 MPa
2610 psi
Compressive Strength 72.0 MPa
10400 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.340 W/m-K

@Temperature 121 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 250 °F
Maximum Service Temperature, Air 250 °C
482 °F
Continuous use
315 °C
599 °F
Shrinkage 0.85 %
0.85 %
Length
3.7 %
3.7 %
Thickness
Electrical Properties Metric English Comments
Volume Resistivity 7.10e+10 ohm-cm
7.10e+10 ohm-cm
Dielectric Strength 1.38 kV/mm
35.1 kV/in
Arc Resistance 260 sec
260 sec