Physical Properties Metric English Comments
Density 17.0 g/cc
0.614 lb/in³
Hogen HM1000 Tungsten-Based Metal
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offe..
Density 17.0 g/cc
0.614 lb/in³
Hogen HM1100 Tungsten-Based Metal
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers hig..
Density 17.0 g/cc
0.614 lb/in³
Mi-Tech Metals HD17 Tungsten-Based Metal
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. ..
Density 17.0 g/cc
0.614 lb/in³
Mi-Tech Metals HD17BB Tungsten-Based Metal
ASTM B-777-07 Class 1; Slightly Magnetic (HD17 is non-magnetic).Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist t..
Density 17.0 g/cc
0.614 lb/in³
Mi-Tech Metals HD17D Tungsten-Based Metal
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The t..
Density 17.0 - 17.6 g/cc
0.614 - 0.636 lb/in³
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Density 17.0 g/cc
0.614 lb/in³
China Tungsten W 90 Tungsten Carbide Powder
Information provided by China Tungsten
Density 17.0 g/cc
0.614 lb/in³
ATI Wah Chang Infiltrated Tungsten (Copper)
Tungsten base infiltrated metal with Copper as infiltrant has been widely used in industry for years. It has proven highly advantageous because of its excellent machinability. Roughly 90% Tungsten a..