Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.79 g/cc | 0.101 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton EXP 36 Cordierite Mullite REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 2.79 g/cc | 0.101 lb/in³ | |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |